a) If requirement for shrinkage of Viscose knitted fabric is less than 5%, it should be used a Free Steam dryer instead of normal stenter. After free steam dryer, material should be sanforazed in a sanforization machine.
b) Material should be in the Process as following;
- Weak Cold Caustification (it can help for better size stabilisation and less creasing of the fabric)
- Dyeing,
- Open width free steam dryer,
- Sanforization.